Fig. 1.

Fig. 2.

Fig. 3.

Parameters of the two-layer discs_
| Set | Layer | Material | Diameter [mm] | Thickness [mm] | Conductivity [MS/m] |
|---|---|---|---|---|---|
| 1 | Upper | Bronze | 59.62 | 2.07 | 6.09 |
| Lower | Brass | 39.92 | 5.12 | 14.22 | |
| 2 | Upper | Bronze | 59.62 | 2.07 | 6.09 |
| Lower | Graphite | 30.15 | 5.02 | 0.52 | |
Changes in the coil impedance ΔZ=Z−Z0 for frequency f=1 kHz and f=10 kHz_
| Set | Freq. f [kHz] | Experiment ΔZ [Ω] | Calculations ΔZ [Ω] | Error ΔR [%] | Error ΔX [%] |
|---|---|---|---|---|---|
| 1 | 1 | 23.18 − j 27.43 | 23.07 − j 27.06 | 0.4 | 1.4 |
| 10 | 256.1 − j 667.1 | 259.0 − j 658.4 | 1.2 | 1.3 | |
| 2 | 1 | 22.05 − j 7.97 | 21.95 − j 7.93 | 0.5 | 0.4 |
| 10 | 310.0 − j 701.5 | 312.3 − j 693.3 | 0.7 | 1.2 |