Table 1
Composition of model alloys (wt%).
| Alloy | Fe3C (%) | W (%) | Ni (%) | Co (%) |
|---|---|---|---|---|
| Fe3C–W–Ni | 85 (1.2%C) | 10 | 5 | — |
| Fe3C–W–Co | 85 (1.2%C) | 10 | — | 5 |
| Fe3C–W–NiCo | 80 (1.2%C) | 10 | 5 | 5 |

Figure 1
Charpy impact specimen and flexural.

Figure 2
SEM image showing the porosity of alloys: (a) Fe3C–W–Ni, (b) Fe3C–W–Co, and (c) Fe3C–W–NiCo.

Figure 3
SEM image by backscattered electrons of phase: (a) Fe3C–W–Ni, (b) Fe3C–W–Co, and (c) Fe3CWNiCo.

Figure 4
EDS elemental maps of the investigated alloys after sintering: (a) 85Fe3C–10W–5Ni, (b) 85Fe3C–10W–5Co, and (c) 80Fe3C–10W–5Ni–5Co alloys.

Figure 5
X-ray diffraction evolution (a) XRD patterns of Fe3C–W-based alloys with Ni, Co, and NiCo binders after sintering at 1400°C compared to the initial powder mixture; (b) diffraction peak shifts in the 43–45° (2θ) range for the (110) plane.

Figure 6
Density evolution before and after sintering.

Figure 7
Microhardness evolution.

Figure 8
The evolution of flexural strength.

Figure 9
The evolution of resilience values.

Figure 10
Charpy V-notched specimens and flexural after impact testing. Mechanical responses of the investigated Fe3CWNi ,Fe3CWCo and Fe3CWNiCo alloys under Charpy impact and three-point bending tests: (a) Charpy impact of Fe3CWNi; (b) Charpy impact of Fe3CWCo; (c) Charpy impact of Fe3CWNiCo; (d) three-point bending of Fe3CWNi; (e) three-point bending of Fe3CWCo and (f) three-point bending of Fe3CWNiCo alloys.

Figure 11
Evolution of the sintering mechanism and phase transformation of Fe3C–W–Ni, Fe3C–W–Co, and Fe3C–W–NiCo alloys. Microstructural evolution and densification behavior of Fe3C-W alloys containing Ni, Co, and NiCo binders after solid-state sintering at 1400 °C: (a, b) Fe3C–W–Ni alloy; (c, d) Fe3C–W–Co alloy; and (e, f) Fe3C–W–NiCo alloy showing advanced densification and microstructural homogeneity.