Table 1:
Mix proportion of concrete specimens
| Material | Vf = 0% | Vf = 0.5% | Vf = 1.0% | Vf = 1.5% |
|---|---|---|---|---|
| W/C | 0.28 | 0.28 | 0.28 | 0.28 |
| Cement (kg/m3) | 732.14 | 732.14 | 732.14 | 732.14 |
| Aggregate (kg/m3) | 920.6 | 920.6 | 920.6 | 920.6 |
| Sand (kg/m3) | 505.18 | 505.18 | 505.18 | 505.18 |
| Water (kg/m3) | 207.05 | 207.05 | 207.05 | 207.05 |
| Steel fibre (kg/m3) | - | 11.9 | 23.7 | 35.5 |
| HRWR (kg/m3) | 7.32 | 7.32 | 7.32 | 7.32 |

Figure 1:
Notched beam specimen geometry

Figure 2:
Test set-up: three-point flexural test

Figure 3:
Meshed 3D model of notched beam (3DNLFEA)

Figure 4:
(a) Compressive strength test results: stress-strain curve; (b) Relationship between peak load and volume fraction (Vf) of steel fibres

Figure 5:
Crack propagation patterns observed in uniaxial compression tests

Figure 6:
Crack propagation patterns observed in notched beam

Figure 7:
Load-displacement curve of notched beams

Figure 8:
Load-CMOD curve of notched beams

Figure 9:
Uniaxial tensile contribution for steel fibre function of the crack mouth opening (CMO)

Figure 10:
Load-displacement curves result for notched beams with varying fibre volume fractions

Figure 11:
Fracturing parameter contour plots for notched beam

Figure 12:
Crack mouth opening displacement (CMOD) contour plots for notched beam