Assessment of fitness for service of Cr-Mo steel tubes in catalytic reforming charge heaters Cover

Assessment of fitness for service of Cr-Mo steel tubes in catalytic reforming charge heaters

By: J. Hucińska and  G. Gajowiec  
Open Access
|Dec 2010

Abstract

In this paper characteristic features of metal dusting corrosion in high temperature gas mixtures of high carbon activity in catalytic reforming units, including Continuous Catalyst Regeneration (CCR) platformer are presented. Examples of 2.25Cr-1Mo and 9Cr-1Mo steel tubes at advanced stages of metal dusting process after long-term service in charge heaters are used to prove that destructive examinations are necessary to provide certain information about possible mechanisms of damage, and are helpful in assessment of immediate fitness for purpose and long-term service capability of the components during and following shut-downs.

DOI: https://doi.org/10.2478/v10077-010-0009-x | Journal eISSN: 2083-4799 | Journal ISSN: 1730-2439
Language: English
Page range: 17 - 26
Published on: Dec 20, 2010
Published by: Gdansk University of Technology
In partnership with: Paradigm Publishing Services
Publication frequency: 4 issues per year

© 2010 J. Hucińska, G. Gajowiec, published by Gdansk University of Technology
This work is licensed under the Creative Commons License.

Volume 10 (2010): Issue 3 (September 2010)