Precipitation of jarosite as a purifying procedure of the solution obtained after leaching of zinc secondary material

Open Access
|Dec 2010

Abstract

Zinc oxide derived from processing of the slime obtained in an industrial process of electrolytic zinc obtaining was leached with the aqueous sulfuric acid solution. The effect of temperature and time on the extent of leaching was determined. The conditions lead to zinc recovery of about 90%. It was found that the extent of arsenic leaching did not depend upon the time and temperature of leaching. Next the conditions of the solution purification procedure were determined. It was found that jarosite formation as well as the degree of arsenic removal is connected with trivalent iron concentration in the solution.

Language: English
Page range: 36 - 39
Published on: Dec 28, 2010
Published by: West Pomeranian University of Technology, Szczecin
In partnership with: Paradigm Publishing Services
Publication frequency: 4 issues per year

© 2010 Andrzej Jarosiński, Artur Przybyła, published by West Pomeranian University of Technology, Szczecin
This work is licensed under the Creative Commons License.

Volume 12 (2010): Issue 4 (December 2010)