Mechanistic Insights into the Long-term Sulphate–chloride Co-exposure Resistance of Self-compacting Engineered Cementitious Composites Cover

Mechanistic Insights into the Long-term Sulphate–chloride Co-exposure Resistance of Self-compacting Engineered Cementitious Composites

Open Access
|Sep 2026
Read online

Figures & tables

Figure 1:

Dog-bone specimens of SC-ECC mixtures under direct tensile test: (a) specimen mounted in the testing machine during loading, and (b) specimen after failure showing the final dominant crack and residual fine cracks within the gauge length

Figure 2:

The experimental program of flowchart summarizing sequence for SC-ECC mixtures, including material selection, specimen casting, curing regime, exposure conditions, and testing schedule. The chart outlines the chronological stages—from material preparation

Figure 3:

Compressive strength testing of SC-ECC specimens: (a) specimens after long-term exposure before testing, (b) experimental setup during compressive loading, and (c) post-failure appearance exhibiting gradual crushing and limited fragmentation, indicative

Figure 4:

Water permeability test setup for SC-ECC specimens under 0.5 MPa hydrostatic pressure, results evaluated according to DIN 1048-5 (1991)

Table 1:

Chloride penetration classification based on total charge passed. ASTM C1202 (2022)

Total charge passed (Coulombs)Chloride penetration classification
<4000High
2000–4000Moderate
1000–2000Low
100–1000Very low
>100Negligible penetration
Figure 5:

Rapid chloride penetration testing of SC-ECC specimens: (a) specimen preparation and surface sealing of 100 × 50 [mm] cylindrical discs before testing, and (b) data acquisition and monitoring of the total charge passed through the specimens

Figure 6:

Half-cell potential testing of SC-ECC specimens: (a) typical test setup showing electrode positioning and electrical connection on the specimen surface, and (b) measurement of corrosion potential using a Cu/CuSO4 reference electrode (CSE)

Figure 7:

Relative compressive strength development of SC-ECC specimens under chloride-only, and combined chloride–sulphate exposure at 28, 90, 180, and 270 days (normalised to 28-day values = 100 %)

Figure 8:

Water penetration depth of SC-ECC specimens exposed to different sulphate concentrations (2.5 %, 5.0 %, and 7.5 % Na2SO4) at 28, 180, and 270 days under partial-immersion conditions. Each value represents the mean of three specimens

Figure 9:

Rapid chloride penetration (RCPT) results of SC-ECC specimens under different sulphate concentrations (2.5–7.5 % Na2SO4) at 56 days. Each value represents the mean of three specimens. The dashed line denotes the ASTM C1202 limit for “very low” chloride Penetration (1000 C)

Table 2:

Half-cell potential results of SC-ECC specimens under different exposure regimes (values in mV vs. CSE; ASTM C876 classification shown in parentheses)

Exposure Condition28 days mean (mV)Corrosion risk classification (ASTM C876) @28d90-day mean (mV)Corrosion risk classification (ASTM C876) @90d180 days (mV)Corrosion risk classification (ASTM C876) @180d270 days (mV)Corrosion risk classification (ASTM C876) @270d
7.5% Na2SO4−205Moderate−217Moderate−235Moderate−252.5Moderate
5% Na2SO4−184Low−196Low−210Low/Moderate−222.5Moderate
2.5% Na2SO4−170Low−182Low−195Low−207.5Low/Moderate
7.5% Na2SO4 + 3% NaCl−340Moderate/High−351Moderate/High−395High−430High/Very high
5% Na2SO4 + 3% NaCl−290Moderate−305Moderate−345Moderate/High−375High
2.5% Na2SO4 + 3% NaCl−270Moderate−285Moderate−317.5Moderate−345Moderate/High
3% NaCl only−230Moderate−248Moderate−277.5Moderate−310Moderate (Near high)
Water (reference)−118Very Low−118Very Low−122.5Low−127.5Low
Figure 10:

Development of half-cell potential of SC-ECC specimens under chloride-only, sulphate-only, and combined chloride–sulphate exposures up to 270 days. The dashed line at −350 mV denotes the ASTM C876 threshold for high corrosion probability

Figure 11:

SEM micrographs of SC-ECC specimens showing microstructural evolution with sulphate concentration and exposure duration: (a) 28-day water-cured reference sample; (b) 2.5 % Na2SO4 — early ettringite nucleation near fibre–matrix interfaces; (c) 5 % Na2SO4 - denser ettringite and gypsum deposits causing local cracking; (d) 7.5 % Na2SO4 — severe matrix deterioration and widened ITZ; (e) high-magnification view of fibre–matrix interphase highlighting partial debonding and secondary deposition

DOI: https://doi.org/10.2478/cee-2026-0079 | Journal eISSN: 2199-6512 (formerly 1336-5835) | Journal ISSN: 1336-5835
Language: English
Page range: 1279 - 1295
Submitted on: Nov 4, 2025
Accepted on: Dec 12, 2025
Published on: Sep 25, 2026
Published by: University of Žilina
In partnership with: Paradigm Publishing Services
Publication frequency: 4 issues per year

© 2026 Mohammed Shaker Amouri, Nada Mahdi Fawzi, published by University of Žilina
This work is licensed under the Creative Commons Attribution 4.0 License.