Skip to main content
Have a personal or library account? Click to login
Experimental Investigation of Eccentric Composite Hollow Steel-Concrete Tensioned Column Cover

Experimental Investigation of Eccentric Composite Hollow Steel-Concrete Tensioned Column

Open Access
|Sep 2026
Read online

Figures & tables

Figure 1:

Reinforced Concrete Tensioned Column

Table 1:

The details of Tested Beams

GroupBeam IDLoaded TypeFailure TypeEccent. (e) [mm]Section TypeLength [mm]Steel Box No.
Group-1C-E-S-1EccentricBalance210Solid500---
C-E-H-2EccentricBalance210Hollow500---
C-E-B-3EccentricBalance210Composite5001
Group-2C-E-B-4Eccentrice < eb190Composite5001
C-E-B-5Eccentrice1 > eb242Composite5001
C-E-B-6Eccentrice2 > eb273Composite5001
C-E-B-7Eccentrice3 > eb305Composite5001
Figure 2:

Geometry and Details of Tested Column

Figure 3:

Reinforcement Details of Tested eccentric column

Figure 4:

Steps for theorical design

Figure 5:

Fabrication the Specimens

Table 2:

Properties of Steel Box

Test IndicationAverage ValueASTM-A 370-10 [14]
Yield Tensile Strength [MPa]325250 Min.
Ultimate Tensile Strength [MPa]436400–500
Table 3:

Properties of reinforced Bars

Test ResultsASTM A 615/A615-22 Grade 60 limits
Bar size [mm]Yield strength [N/mm2]Ultimate strength [N/mm2]Elongation [%]Yield strength Min. [N/mm2]Ultimate strength Min. [N/mm2]Elongation [%]
10619638244205509
12577.665311.63505507
Table 4:

Mix Proportions for Fresh Concrete

Cement [kg/m3]Sand [kg/m3]Gravel [kg/m3]Water [kg/m3]
410813955196
Table 5:

Mechanical Properties of the concrete

Sample No.Cylinderical Compressive strength (fc′) [MPa]Tensile Strength
Splitting [MPa]Modulus of Rupture [MPa]
124.22.53.31
224. 12.23.45
323.62.63.67
Average24.002.433.48
Figure 6:

Testing layout

Figure 7:

Theorical Design Information

Table 6:

Theoretical and Experimental Tensile Loads, Moments and Eccentricities

G. IDBeamTheoretical ResultsExperimental Results(Pu/Pn) ×100%(Mu/Mn) ×100%
Force (Pn) [kN]Moment (Mn) [kN.m]Eccent. (e) [mm]Force (Pu) [kN]Moment (Mu) [kN.m]Eccent. (e) [kN.m]
G- 1C-E-S-1136.7728.8021112526.2521091.3991.16
C-E-H-2136.0228.5821012025.221088.2288.16
C-E-B-3156.9232.9621013527.321086.0382.84
G-2C-E-B-4169.3432.2419014026.619082.6782.50
C-E-B-5144.2734.8624212530.2524286.6486.77
C-E-B-6126.4834.6227411531.5127490.9391.00
C-E-B-7112.7534.3930510030.530588.6988.68
Average88 %89 %
Figure 8:

Theoretical and Experimental Tensile Forces and Moments

Table 7:

First Crack Load and Deflection

Group IDBeamPcr [kN]Pu [kN](Pcr/Pu) ×100%Crack TypeMid-Span Deflection [mm]
Group 1C-E-S-14512536 %Direct6
C-E-H-24612038 %Direct6.1
C-E-B-35013537%Direct6.5
Group 2C-E-B-44714034 %Direct5.7
C-E-B-55012540 %Direct6.3
C-E-B-64811542 %Direct6.8
C-E-B-74310043 %Direct7
Figure 9:

Modes of failure

DOI: https://doi.org/10.2478/cee-2026-0061 | Journal eISSN: 2199-6512 (formerly 1336-5835) | Journal ISSN: 1336-5835
Language: English
Page range: 1037 - 1049
Submitted on: Aug 31, 2025
Accepted on: Nov 20, 2025
Published on: Sep 25, 2026
Published by: University of Žilina
In partnership with: Paradigm Publishing Services
Publication frequency: 4 issues per year

© 2026 Wameedh Issa Braidi, Rasool Dakhil Mohsin, Nasser Hakeem Tu’ma, Haider Abdul-Kareem Raheem, published by University of Žilina
This work is licensed under the Creative Commons Attribution 4.0 License.