Figure 1:
Systematic Research for Literature Review

Figure 2:
PRISMA Flowchart for Sample Searching
Table 1:
Overview of Functional Units Commonly Used in Life Cycle Assessment (LCA) Studies of Recycled Aggregate Concrete (RAC), Highlighting Their Defining Parameters, Application Contexts, and Limitations
| Designation | Functional Unit | Description |
|---|---|---|
| RCU1 | Volume-based assessment | Evaluates the environmental impact per cubic meter of RAC compared with an equivalent volume of natural aggregate concrete NAC, considering varying levels of aggregate replacement. (Bandeira et al.; Jin et al., 2024; Epstein, 2018) |
| RCU2 | Volume and strength combined | Uses 1.5 m3 of concrete as the basis, with mix proportions adjusted to ensure comparable compressive strength between NAC and RAC, often requiring additional cement in RAC mixes. (Oyedele et al., 2013; Serres et al., 2016; Won et al., 2016) |
| RCU3 | Strength-to-impact ratio fcm/GWP | Compares the ratio of mean compressive strength to global warming potential GWP across RAC and NAC mixtures to evaluate efficiency and environmental benefit. (Teh et al., 2017; Khanh and Kim, 2015) |
| RCU4 | Functional performance and durability | Compares RAC and NAC, assuming equal strength, workability, and performance in non-aggressive environments; considers lifecycle equivalence in structural applications. (Lu et al., 2018; Van der Zee and Zeman, 2016) |
| RCU5 | Integrated strength-lifetime index | Evaluates the quantity of concrete required to achieve a defined strength e.g., 1.65 MPa over a specific service life e.g., one year, providing a composite measure for LCA analysis. (Jin et al., 2017; Colangelo et al., 2018; Borghi et al., 2018) |

Figure 3:
Processing of Recycled Aggregates
Table 2:
Comparison of Physical and Mechanical Properties of Natural Aggregates NA and Recycled Coarse Aggregates RCA
| Property | Natural Aggregate NA | Recycled Coarse Aggregate RCA |
|---|---|---|
| Bulk Density [kg/m3] | 2600–2700 | 2100–2400 |
| Water Absorption [%] | 0.5–2.0 | 5.0–8.0 |
| Aggregate Crushing Value ACV, [%] | 20–25 | 25–35 |
| Modulus of Elasticity [GPa] | 30–40 | 18–26 |
| Abrasion Resistance LA Abrasion, [%] loss | 20–25 | 30–40 |
Table 3:
Comparative Behavioural Performance of Natural Aggregate Concrete and RCA Concrete
| Property | NA Concrete | RCA Concrete |
|---|---|---|
| Slump [mm] | 75–100 | 50–75 without adjustment |
| Water Absorption [%] | 0.5–2.0 | 5.0–8.0 |
| Compressive Strength [MPa] | 35–55 | 28–50 at 28 days, depending on %RCA |
| Tensile Strength [MPa] | 2.8–4.5 | 2.0–3.8 |
| Modulus of Elasticity [GPa] | 30–40 | 18–26 |
| Water Permeability [m/s] | <1×10−11 | >3×10−11 |
| Drying Shrinkage [µε] | 400–600 | 500–800 |
| Chloride Diffusion [10−12 m2/s] | 1.0–2.0 | 2.5–4.5 |
| Creep Strain at 90 days, [µε] | 1200–1800 | 1500–2400 |

Figure 4:
Road Map for Mortar Treatment Process
Table 4:
Comparison of 28-Day Average Strength Properties of Recycled Aggregate Concrete (RAC) at Varying Replacement Levels
| Strength Type | Natural Aggregate Concrete | RCA Concrete 20–50% RCA | RCA Concrete ≥50% RCA |
|---|---|---|---|
| Compressive Strength [MPa] | 40–60 | 35–48 | 28–40 |
| Tensile Strength [MPa] | 3.0–4.5 | 2.5–3.8 | 2.0–3.2 |
| Flexural Strength [MPa] | 4.5–6.0 | 4.0–5.4 | 3.5–5.0 |

Figure 5:
Modulus of Elasticity with RCA Replacement Graph
Table 5:
Structural Performance Comparison: NA vs. RCA Concrete Elements
| Structural Element | Metric | NA Concrete | RCA Concrete ≤50% |
|---|---|---|---|
| Beam Flexure (Tamayo et al., 2019) | Ultimate Moment [kNm] | 78–85 | 72–80 |
| Beam Shear (Xiao Jiabin et al., 2006) | Shear Load [kN] | 40–50 | 35–45 |
| Column Axial (Wu Xu et al., 2011) | Ultimate Load [kN] | 550–600 | 470–520 |
| Crack Width (Xiao Jiabin et al., 2006) | At Ultimate Load [mm] | 0.6–0.9 | 0.8–1.2 |

Figure 6:
Comparison of Ultimate Load Capacities for NA and RCA Concrete in Structural Elements
Table 6:
Structural Application Guidelines for Recycled Concrete Aggregate (RCA) in Reinforced Concrete - Recommended Use Based on Replacement Levels, Mechanical Performance, and Durability Considerations
| RCA Replacement Level | Mechanical Performance | Durability | Recommended Application |
|---|---|---|---|
| 0–30% | Minor reductions <10% | Comparable to NA concrete | All reinforced concrete general use |
| 30–50% | Moderate loss 10–20% | Acceptable with SCMs | Beams, slabs, secondary structural elements |
| 50–100% | Significant strength reduction | High permeability risk | Pavements, foundations, non-structural use |

Figure 7:
Strength Reduction Trend with Increasing RCA Replacement Percentage
Table 7:
Design Considerations for Recycled Concrete Aggregate (RCA) Mixes
| Concrete Type | Water Absorption [%] | Permeability [m/s] | Durability Class |
|---|---|---|---|
| Natural Aggregate NAC | 2.3–2.8 | 8.5 × 10−12 | High |
| RCA Untreated | 5.0–6.2 | 1.5–2.2 × 10−11 | Low to Medium |
| RCA Treated + SCM | 3.2–4.1 | 9.5–1.2 × 10−11 | Medium to High |
Table 8:
Durability Parameters of NA Concrete and RAC with and without Treatment or SCMs
| Parameter | NA Concrete | RAC Untreated | RAC Treated + SCMs |
|---|---|---|---|
| Chloride Diffusion m2/s (Jiang et al., 2024) | 1.0 × 10−12 | 1.7–2.9 × 10−12 | 1.2–1.8 × 10−12 |
| Carbonation Depth 28 days (Possan et al., 2017) | 5.6 mm | 8.5–9.2 mm | 6.3–7.0 mm |
| Suggested RCA (Verma et al., 2023) | — | ≤30% | ≤50% with SCMs |
Table 9:
Performance Comparison of Natural Aggregate Concrete (NAC), Untreated Recycled Aggregate Concrete (RAC), and Treated RAC with Supplementary Cementitious Materials (SCMs)
| Parameter | NAC | RAC Untreated | RAC Treated + SCMs |
|---|---|---|---|
| Freeze–Thaw Scaling kg/m2, 300 cycles | 0.3–0.6 | 0.7–1.0 | 0.4–0.6 |
| Sulfate Expansion % | <0.10% | 0.13–0.18% | 0.09–0.12% |
Table 10:
Long-Term Deformation Characteristics of Natural Aggregate Concrete (NAC) and Recycled Aggregate Concrete (RAC)
| Property | NAC | RAC Untreated | RAC Treated/SCM |
|---|---|---|---|
| Drying Shrinkage [με] | 620–680 | 850–950 | 700–800 |
| Creep Coefficient [-] | 1.8–2.2 | 2.5–3.0 | 2.1–2.4 |
| Microcrack Density | Low | Moderate to High | Moderate |
Table 11:
Comparative Evaluation of Mix Design Methods for Recycled Aggregate Concrete (RAC)
| Mix Design Approach | Workability | Strength | Durability | Recommended RCA Level [%] |
|---|---|---|---|---|
| Volume-Based Substitution (Fathifazl et al., 2009) | Poor | Moderate | Poor | ≤30 |
| Equivalent Mortar Volume (Fathifazl et al., 2009) | Good | High | High | ≤50 |
| Particle Packing Optimization (Pepe et al., 2016) | Very Good | High | High | ≤100 |
| SCM-Enhanced Mix (Jain et al., 2021) | Good | High | Very High | ≤50 |
Table 12:
Environmental Impact Indicators of Different Concrete Types
| Concrete Type | GWP [kg CO2-eq/m3] | CED [MJ/m3] |
|---|---|---|
| Natural Aggregate NAC | 320–360 | 2600–2800 |
| RAC 50% RCA | 275–300 | 2000–2300 |
| RAC + SCMs | 220–260 | 1700–2100 |

Figure 8:
Carbonation Sequestration Trend of RCA
Table 13:
Key Barriers to RCA Adoption and Corresponding Solutions
| Barrier | Root Cause | Recommended Solution |
|---|---|---|
| Regulatory uncertainty (Ferrandez et al., 2023) | Lack of harmonized design codes | National standardization and international benchmarking |
| Quality variability (Silva et al., 2017; Brito et al., 2019) | Source heterogeneity, lack of RCA-specific specs | Treatment protocols and RCA grading systems |
| Industry resistance (Piccinali et al., 2025) | Negative perception and risk aversion | Demonstration projects, training, and knowledge transfer |
| Economic and logistical hurdles (Dinh, 2023) | High processing costs, erratic supply | Incentivization schemes, regional recycling networks |

Figure 9:
Adoption Challenges of RCA