Fig. 1
Photograph of LA-ZTC crystals.

Fig. 2
(a) EDS spectrum of LA-ZTC crystal, (b) SEM micrograph of LA-ZTC crystal.

Fig. 3
(a) Load dependent hardness (b) logP vs. logd.
Table 1
Hardness parameters of LA-ZTC crystal.
| Load [g] | VHN [kG/mm2] | C11 [GPa] | σy [Pa] |
|---|---|---|---|
| 15 | 17.2 | 2.49 × 105 | 6020510 |
| 25 | 26.79 | 5.41 × 105 | 9377294 |
| 50 | 33.98 | 8.20 × 105 | 11894007 |

Fig. 4
Plot of SHG output intensity.
Table 2
Optical resolution of Z-scan setup.
| Parameters | Magnitude |
|---|---|
| Laser wavelength (λ) | 632.8 nm |
| Laser power (P) | 10 mW |
| Lens focal length (f) | 20 cm |
| Optical path distance (Z) | 113 cm |
| Beam waist radius (ωa | 1 mm |
| Aperture radius (ra) | 1.5 mm |
| Incident intensity at the focus (Io) | 2.3375 KW/m2 |

Fig. 5
Z-scan transmittance curve with (a) closed and (b) open aperture.
Table 3
TONLO parameters of LA-ZTC crystal.

Fig. 6
Temperature dependent (a) dielectric constant, (b) dielectric loss.