Have a personal or library account? Click to login
Production of ZnO and CdO-ZnO thin Films by Extraction–Pyrolytic Method Cover

Production of ZnO and CdO-ZnO thin Films by Extraction–Pyrolytic Method

Open Access
|Jul 2016

Abstract

The extraction-pyrolytic method has been applied to produce the ZnO and CdO-ZnO thin films on glass and quartz glass substrates. According to X-ray diffraction measurements, the ZnO and CdO phases have been produced with an average size of crystallites about 8–42 nm in the films. The thickness of the layers measured by a profilometer has been up to 150 nm. The surface morphology measurements show that the surface of the films may be rough and non-continuous. The SEM results confirm the dependence between the preparation procedure and the quality of the thin film.

DOI: https://doi.org/10.1515/lpts-2016-0021 | Journal eISSN: 2255-8896 | Journal ISSN: 0868-8257
Language: English
Page range: 57 - 66
Published on: Jul 27, 2016
Published by: Institute of Physical Energetics
In partnership with: Paradigm Publishing Services
Publication frequency: 6 issues per year

© 2016 A. Cvetkovs, O. Kiselova, U. Rogulis, V. Serga, R. Ignatans, published by Institute of Physical Energetics
This work is licensed under the Creative Commons Attribution-NonCommercial-NoDerivatives 3.0 License.