Have a personal or library account? Click to login
Developing the inoculation procedure for high-quality cast iron with flake graphite, intended for large-size casting (bottom or distance plates and counterweights) – produced in Krakodlew Foundry S.A.
Benedetti, M., Torresani, E., Fontanari, V., & Lusuardi, D. (2017). Fatigue and Fracture Resistance of Heavy-Section Ferritic Ductile Cast Iron. Metals, 7(3), 88. https://doi.org/10.3390/met7030088
Dobrovska, J., Kavicka, F., Stransky, K., Sekanina, B., Stetina, J., Barlat, F., Moon, Y.H., & Lee, M.G. (2009). Numerical Optimization of the Method of Cooling of a Massive Casting of Ductile Cast-Iron. Materials and Technology, 43, 73–78. https://doi.org/10.1063/1.3457606
Gilewski, R., Kopyciński, D., Guzik, E., & Szczęsny, A. (2021). An Evaluation of the Microstructure of High-Aluminum Cast Iron in Terms of the Replacement of Aluminum Carbide with Titanium Carbide or Tungsten Carbide. Applied Sciences, 11(20), 9527. https://doi.org/10.3390/app11209527
Kopyciński, D., Siekaniec, D., Szczęsny, A., Sokolnicki, M., & Nowak, A. (2016). The Althoff-Radtke test adapter for high chromium cast iron. Archives of Foundry Engineering, 26(4), 74–77.
Mourad, M.M., El-Hadad, S., Ibrahim, M., & Nofal, A. (2015). Effect of Processing Parameters on the Mechanical Properties of Heavy Section Ductile Iron. Journal of Metallurgy, 1–11. https://doi.org/10.1155/2015/931535
Tęcza, G., & Zapała, R. (2018). Changes in impact strength and abrasive wear resistance of cast high manganese steel due to the formation of primary titanium carbides. Archives of Foundry Engineering, 18(1), 119–122. https://doi.org/10.24425/118823
Wang, Q., Cheng, G., & Hou, Y. (2020). Effect of Titanium Addition on As-Cast Structure and High-Temperature Tensile Property of 20Cr-8Ni Stainless Steel for Heavy Castings. Metals, 10, 4–15. https://doi.org/10.1016/j.msea.2006.09.001
Wang, Q, Chen, S., & Rong, L. (2020). δ-Ferrite Formation and Its Effect on the Mechanical Properties of Heavy-Section AISI 316 Stainless Steel Casting. Metallurgical and Materials Transactions, 51(6), 2998–3008. https://doi.org/10.1007/s11661-020-05717-0