CuO as sintering additive to Sr0.4Ca0.6La4Ti5O17 ceramics Cover

CuO as sintering additive to Sr0.4Ca0.6La4Ti5O17 ceramics

By: A. Manan,  L. Shah and  Attaullah  
Open Access
|Feb 2013

Abstract

The effects of CuO addition on the sintering behavior and microwave dielectric properties of Sr0.4Ca0.6La4Ti5O17 ceramics were investigated. CuO was selected as a liquid phase sintering aid to lower the sintering temperature of Sr0.4Ca0.6La4Ti5O17 ceramics. With CuO addition, the sintering temperature of Sr0.4Ca0.6La4Ti5O17 ceramics was effectively reduced from 1550 °C to 1475 °C. The crystalline phase exhibited no phase difference and no second phase was detected at all addition levels. The electric permittivity was not significantly affected by various amounts of CuO addition and ranged from 52 to 54. Small values (<+7 ppm/K) of the temperature coefficient of resonant frequency were obtained for Sr0.4Ca0.6La4Ti5O17 ceramics. However, the unloaded quality factor Q u was strongly dependent upon the CuO concentration. Q u f o ∼ 10500 GHz was obtained for Sr0.4Ca0.6La4Ti5O17 ceramics with 0.5 wt.% of CuO addition, sintered at 1475 °C.

DOI: https://doi.org/10.2478/s13536-012-0074-4 | Journal eISSN: 2083-134X | Journal ISSN: 2083-1331
Language: English
Page range: 122 - 125
Published on: Feb 9, 2013
Published by: Wroclaw University of Science and Technology
In partnership with: Paradigm Publishing Services
Publication frequency: 4 issues per year

© 2013 A. Manan, L. Shah, Attaullah, published by Wroclaw University of Science and Technology
This work is licensed under the Creative Commons Attribution-NonCommercial-NoDerivatives 3.0 License.