2. SHI, F., WANG, L., CUI, W., LIU, C. 2008. Precipitation Kinetics of Cr2N. In High Nitrogen Austenitic Stainless Steel. Journal of iron and steel research, International, 15(6), 72-77.
3. RONCERY, L.M., WEBER, S., THEISEN, W. 2011. Nucleaton and Precipitaion kinetics of M23C6 and M2N in an Fe- Mn- Cr- C-N austenitic matrix and their relationshiop with the sensitization phenomenon. Acta Materialia, 69, 6275-6286.
4. HAZLINGER, M., MORAVČÍK, R., ČAPLOVIČ, Ľ. 2007. Degradačné procesy a predikcia životnosti. E-skriptum. Trnava: AlumniPress, 2007, 162 p. ISBN 978-80-8096-031-5
6. DOMÁNKOVÁ, M. 2008. Relationship between microstructure and corrosion properties of chosen austenitic stainless steel. Dresden: Forschungszentrum Dresden. ISBN 978-3-941405-01-1
8. KNUTSEN, R.D., LANG, C.I., BASON, J.A. 2004. Discontinuous cellular precipitation in Cr-Mn-N steel with niobium and vanadium additions. In Acta materialia, 52, 2407-2417.
10. MA, Y., RONG, F., ZHOU, R., LANG, Y., JIANG, Y. 2007. Study of Precipitation of High Nitrogen Containing Austenitic Stainless Steel During Isotermal Aging At Intermediate Temperature. In Proceeding of Sino- Swedish Materials Symposium.10.1016/S1006-706X(08)60108-9
12. ASTM A262 - 14 Standard Practices for Detecting Susceptibility to Intergranular Attack in Austenitic Stainless Steels, Annual Book of ASTM Standards, Vol. 03.02, ASTM International, West Conshohocken, PA.