- Bitondo, C., Bossio, A., Monetta, T., Curioni, M., Bellucci, F., 2014. The effect of annealing on the corrosion behaviour of 444 stainless steel for drinking water applications. Corrosion science, 87, 6-10.
- Chen, X., Li, J., Cheng, X., Wang, H., Huang, Z., 2018. Effect of heat treatment on microstructure, mechanical and corrosion properties of austenitic stainless steel 316L using arc additive manufacturing. Materials Science and Engineering: A., 715, 307-314.
- Chen, X., Liu, H., Sun, X., Zan, B., Liang, M., 2021. Chloride corrosion behavior on heating pipeline made by AISI 304 and AISI 316 in reclaimed water. RSC Advances, 11, 61, 38765-38773.
- Cleaning and Descaling Stainless Steels. A Designers’ Handbook Series N° 9001, Available online: https://nickelinstitute.org/media/4399/cleaning-and-descaling-stainless-steel-9001-updated.pdf (accessed on 18 June 2024).
- Chvalníková, V., Uhríčik, M., Palček, P., Slezák, M., Šikyňa, L., Drímalová, P., 2023. Austenitic steel AISI 304 under static and cyclic loading. ManufacturingTechnology, 23, 5, 623-629.
- Dastgerdi, A.A., Brenna, A., Ormellese, M., Pedeferri, M.P., Bolzoni, F., 2019. Experimental design to study the influence of temperature, pH, and chloride concentration on the pitting and crevice corrosion of UNS S30403 stainless steel, Corrosion Science 159, 108160.
- Donik, Č., 2011. Surface characterization and pickling characteristics of the oxide scale on duplex stainless steel. Materials and technology, 45, 4, 329-333.
- Elshawesh, F., Elhoud, A., 2004. Role of heat tint on pitting corrosion of 304 austenitic stainless steel in chloride environment. Proceedings of EUROCORR - Prevision a Long Terme et Modelisation de la Corrosion, Nice, France, 12–16 September 2004.
- Glass, J., 2010. Sustainability of construction materials. International Journal of Sustainable Engineering, 3, 1, 65.
- Ha, H.Y., Lee, T.H., Bae, J.H., Chun, D.W., 2018. Molybdenum Effects on Pitting Corrosion Resistance of FeCrMnMoNC Austenitic Stainless Steels. Metals, 8, 8, 653.
- He, V., Guo, Y.J., Wu, X.Y., Jiang, Y.M., Li, J., 2016. Effect of Solution Annealing Temperature on Pitting Behavior of Duplex Stainless Steel 2204 in Chloride Solutions. Journal of Iron and Steel Research International, 23, 4, 357-363.
- Ibrahim, M.A.M., Abd El Rehim, S.S., Hamza, M.M., 2009. Corrosion behavior of some austenitic stainless steels in chloride environments. Materials Chemistry and Physics, 115, 1, 80-85.
- Kuchariková, L., Liptáková, T., Tillová, E., Kajánek, D., Schmidová, E., 2018. Role of Chemical Composition in Corrosion of Aluminum Alloys. Metals, 8, 581.
- Kumar, V., Gupta, R.K., Das, G., 2020. Influence of Deformation and Annealing on Microstructure and Corrosion Behavior of Austenitic Stainless Steel. Materials Today-Proceedings, 22, 4, 3347-3352.
- Lai, J.K.L., Lo, K.H., Shek, C.H., 2012. Austenitic stainless steel. In: Stainless steels: An introduction and recent developments. Bentham Science Publexecutive STE Y-2, Sharjah, U Arab Emirates.
- Li, Y., Qiu, J., Zhao, J., Ye, Q., Zhu, Y., Mao, J., 2018. Enhancement of Pitting Corrosion Resistance of Austenitic Stainless Steel Through Deposition of Amorphous/Nanocrystalline Oxy-nitrided Phases by Active Screen Plasma Treatment. Materials Research, 21, 6.
- Liu, W., Yang, H., Li, X., Zhang, Z., Lin, Y., Deng, K., 2022. Effect of Chloride and Iodide on the Corrosion Behavior of 13Cr Stainless Steel. Metals, 12, 11, 1833.
- Njoku, R.E., Obikwelu, D.N., Ugwuoke, B., Ocheri, C., 2023. Investigation of Solution Annealing Treatment Effect on Corrosion Resistance of AISI 304 Austenitic Stainless Steel for Oil Industry Application. Nanotechnology & Applications, Available online: https://www.scivisionpub.com/pdfs/investigation-of-solution-annealing-treatment-effect-on-corrosion-resistance-of-aisi-304-austenitic-stainless-steel-for-oil-indust-2749.pdf (accessed on 25 October 2024).
- Ofuyekpone, O., Amaechi, C. and Utu, O.G., 2015. Effect of Solution Annealing Temperature on the Microstructure and Mechanical Properties of AISI 304L. International Journal of Applied Research and Technology, 4, 4, 65–75.
- Padilha, A., Lesley, R., Rios, P.R., 2007. Stainless steels heat treatment (Chapter 12). In: Steel Heat Treatment Handbook (Second Edition). Boca Raton: CRC Press, 695-739.
- Pei, W., Yang, S., Cao, K., Zhao, A., 2023. Effect of Annealing Temperature on Mechanical Properties andWork Hardening of Nickel-Saving Stainless Steel. Materials, 16, 3988.
- Ramírez, J., Berrio, E., Alvarado-Avila, M.I., Field, D., Onate, A., Sanhueza, J.P., Montoya, L.F., Meléndrez, M.F., Rojas, D., 2023. Effect of solution annealing temperature on the localised corrosion behaviour of a modified super austenitic steel produced in an open-air atmosphere. Materials Chemistry and Physics, 299, 127498.
- Rustandi, A., Setiawan, S., Fathurrahman, I., 2017. The Effect of Sodium Chloride Concentration on Corrosion Resistance of Austenitic Stainless Steel 316L and SMA Weldment. Solid State Phenomena, 263, 120-124.
- Szewczyk-Nykiel, A., 2015. The influence of molybdenum on corrosion resistance of sintered austenitic stainless steels. Technical Transactions, 4, 131-142.
- Szklarska-Smialowska, Z., 2005. Pitting and Crevice Corrosion. Houston: NACE International: Houston.
- Upadhyay, N., Shankar, A.R., Balakrishnan, A., George, R.P., Pujar, M.G., Philip, J., Amarendra, G., 2020. Effect of Molybdenum on Pit Initiation Rate and Pit Growth Using Electrochemical Noise and Its Correlation with Confocal Laser Scanning Microscopic Studies. Journal of Materials Engineering and Performance, 29, 5337-5345.
- Wu, B., Li, N., Zhang, Y., Ming, H., Shu, M., Sun, Y., Hou, D., Li, Y., Wang, J., Han, E.H., 2024. Effect of solution annealing and Al addition on the corrosion behavior of austenitic stainless steel in supercritical carbon dioxide at high temperature. Corrosion Science, 234, 112131.
- Zhang, C., Wei, Y., Yang, J., Emori, W., Li, J., 2020. Effects of nitric acid passivation on the corrosion behavior of ZG06Cr13Ni4Mo stainless steel in simulated marine atmosphere. Materials and Corrosion, 71, 9, 1576-1590.