Have a personal or library account? Click to login

Mechanical properties evaluation and ultrasound diagnosis of unsaturated polyester-glass pipes

Open Access
|Jun 2015

References

  1. 1. Janson, L.E. (December, 1993). Method for tightness testing of plastics pressure pipelines. Constr. Build. Mater. 7(4), 241-244. DOI: 10.1016/0950-0618(93)90008-Z.10.1016/0950-0618(93)90008-Z
  2. 2. Hearn, G.L. (March 2002). Electrostatic ignition hazards arising from fuel fl ow in plastic pipelines. J. Loss Prevent. Proc. 15(2), 105-109. DOI:10.1016/S0950-4230(01)00061-4.10.1016/S0950-4230(01)00061-4
  3. 3. Marsh, G. (March 2006). Composites keep pipelines fl owing. Reinf. Plast. 50(3), 34-36. DOI: 10.1016/S0034-3617(06)70940-7.10.1016/S0034-3617(06)70940-7
  4. 4. Jones, R.M. (1998). Mechanics of composite materials (2nd ed.). Philadelphia, USA: Taylor & Francis Press.
  5. 5. Królikowski, W., Kłosowska-Wołkowicz, Z. & Penczek P. (1986). Resin and polyester and laminates (2nd ed.). Warsaw, Poland: WNT Press. (In Polish).
  6. 6. German, J. (1996). The basis of mechanics of fi bers composites: a scripts for the students of higher technical schools. Cracow, Poland: Cracow University of Technology Publishing. (In Polish).
  7. 7. Hull, D., Clyne, T.W. (1996). An introduction to composite materials. Melbourne, Australia: Cambridge University Press.10.1017/CBO9781139170130
  8. 8. Błażejewski, W. (2007). The application of acoustic emission in comparative research of braid carriers of composite bottles. In Wróbel G. Polymers and composites construction. Cieszyn, Poland: Logos Press Publishing (In Polish).
  9. 9. Czulak, A. (2010). Shaping of the structure and properties of the fi ber glass-woven composite pipe element, Unpublished doctoral dissertation. Technishe University of Dresden, Germany.
  10. 10. Błażejewski, W. (2009). Methodology of selection of the structure of composite braid carriers with reference to containers made by the winding method. Tech. Transactions - Mechanics z. 1-M, 9-14. (In Polish).
  11. 11. Cohen, D. (1997, July). Infl uence of fi lament winding parameters on composite vessel quality and strength, Comp.: Part A, 28A, 1035-1047. DOI: 10.1016/S1359-835X(97)00073-0.10.1016/S1359-835X(97)00073-0
  12. 12. Deputat, J. (1997). Non-destructive methods of research on materials properties. Warsaw, Poland: Biuro Gamma Press (In Polish).
  13. 13. Śliwiński, A. (2001). Physics for industry. Ultrasounds and their applications (2nd ed). Warsaw, Poland: WNT Press (In Polish).
  14. 14. Kozień, M.S. (2005). Hybrid Method of Evaluation of Sounds Radiated by Vibrating Surface Elements, J. Theor. Appl. Mech. 43,1, 119-133 (In Polish).
  15. 15. Lewińska-Romicka, A. (2001). Non-destructive research. The basis of defectoscopy. Warsaw, Poland: WNT Press (In Polish).
  16. 16. Ostachowicz, W., Wandowski, T., Malinowski, P. (2008). Elastic Wave Phased Array for Damage Localisation, J. Theor. Appl. Mech. 46, 917-931. (In Polish).
  17. 17. Wróbel, G. (2008). Non-destructive methods of engineer research on polymer materials. Gliwice, Poland: Silesian University of Technology Publishing, (In Polish).
  18. 18. Rojek, M., Szymiczek, M., Wróbel, G. (2011). Non-destructive methods of research on polymer materials, Plast. Proces. 6(144), 507-510 (In Polish).
  19. 19. Rojek, M. (2011): Methodology of diagnostics research of layered composite materials with polymer warp. Gliwice, Poland: International OCSCO World Press (In Polish).
  20. 20. Martin, R. (2008). Ageing of composites, Cambridge, England: Woodhead Publishing Limited.
  21. 21. Bogdan-Włodek, A., Kozioł, M. & Myalski, J. (April, 2012). Influence of surface treatment on the wetting process of jute fi bres with thermosetting polyester resin. Pol. J. Chem. Tech. 14,1, 21-27. DOI: 10.2478/v10026-012-0054-9.10.2478/v10026-012-0054-9
  22. 22. Landowski, M., Budzik, M. & Imielińska, K. (March, 2011). On degradation of glass/polyester laminate immersed in water. Advan. Mater. Sci. 11, 1, 35-39. DOI: 10.2478/v10077-011-004-x.
  23. 23. Harris, B. (2003). Fatigue in composites, Cambridge, England: Woodhead Publishing Limited.
  24. 24. Szymiczek, M., Rojek, M. & Wróbel, G. (2011).Test of composite pipe in the aspect of diagnostic of aging - fatigue changes. Proceedings of International Seminar on Science and Education, 16-23 April 2011(pp. 61-63). Rome, Italy.
  25. 25. Stabik, J., Szymiczek, M., Wróbel, G. & Rojek, M. (2012). New stand for composite pipes testing. Proceedings of X International Conference of the Quality, Reliability and Long Usage of Technical Systems and Technological Processes, 20-27 November 2012 (pp. 63-66), Eilat, Israel.
  26. 26. Szymiczek, M., Wróbel, G., M. Rojek, M. & Czapla T. (2013). Simulation diagnostics of the polyester-glass pipes degradation process; experimental basis, J. Achievements Mater. Manufact. Engineer., 59/1, 37-47.
  27. 27. Standards Association of Poland (2002). Poland standard: Plastics piping - Glass-reinforced thermosetting plastics (GRP) pipes - Determination of the apparent initial circumferential tensile strength. PN-EN 1394-2002.
  28. 28. Standards Association of Poland (1993). Poland standard: Plastics - Determination of fl exural properties. PN-EN ISO 178-1993.
Language: English
Page range: 77 - 83
Published on: Jun 9, 2015
Published by: West Pomeranian University of Technology, Szczecin
In partnership with: Paradigm Publishing Services
Publication frequency: 4 issues per year

© 2015 Gabriel Wróbel, Maciej Rojek, Małgorzata Szymiczek, published by West Pomeranian University of Technology, Szczecin
This work is licensed under the Creative Commons Attribution-NonCommercial-NoDerivatives 3.0 License.