Possible Applications of Hardening Slurries with Fly Ash from Thermal Treatment of Municipal Sewage Sludge in Environmental Protection Structures Cover

Possible Applications of Hardening Slurries with Fly Ash from Thermal Treatment of Municipal Sewage Sludge in Environmental Protection Structures

Open Access
|Sep 2016

References

  1. BN-90/1785-01 (1990) Drilling Fluids. The field test methods (in Polish).
  2. Borys M. (2012) Antifiltration barriers from hardening suspensions in corps and substratum of flood control banks, Wiadomosci melioracyjne i łakarskie, 2 (433), 89-95 (in Polish).
  3. Central Statistical Office of Poland. Environmental Protection (2004-2014) (in Polish).
  4. Falacińnski P. (2011) Leak Tightness of hardening slurries with fluidal fly ashes in chemically aggressive environments, Archives of Environmental Protection, PolishAcademy of Sciences, 37 (1), 115-134.
  5. Falaciński P. (2012) Possible applications of hardening slurries with fluidal fly ashes in environment protection structures, Archives of Environmental Protection, Polish Academy of Sciences, 38 (3), 91-104.10.2478/v10265-012-0031-7
  6. Kledyński Z., Rafalski L. (2009) Hardening slurries, Warszawa, KILiW PAN, IPPT PAN (in Polish).
  7. Kłosiński B. (2003) Technical conditions for execution diaphragm walls, Wydawnictwo Instytut Badawczy Dróg i Mostów, Seria I, Informacje, instrukcje, z. 35, Warszawa (in Polish).
  8. Łukawska M. (2014) Speciation analysis of phosphorus in sewage sludge after thermal utilization of sludge, Inzynieria i Ochrona Srodowiska, 17 (3), 433-439 (in Polish).
  9. Małolepszy J., Tkaczewska E. (2006) The influence of fly ash from co-firing of coal and biomass on hydration process and properties of cement, Materiały konferencji Dni Betonu.Wisła, 591-601 (in Polish).
  10. Pająk T. (2014) Thermal treatment of sewage sludge and the challenges of year 2016, Inzynieria i Ochrona Srodowiska, 17 (3), 363-376 (in Polish).
  11. PN-85/G-02320 (1985) Drilling. Cements and cement pastes for cementing of boreholes (in Polish).
  12. PN-EN 12390-3 (2011) Testing hardened concrete - Part 3: Compressive strength of test specimens (in Polish).
  13. PN-EN 12390-6 (2011) Testing hardened concrete - Part 6: Tensile splitting strength of test specimens (in Polish).
  14. PN-EN 12390-7 (2011) Testing hardened concrete - Part 7: Density of hardened concrete (in Polish).
  15. PN-EN 1538+A1 (2015-08) Execution of special geotechnical works - Diaphragm walls (in Polish).
  16. Rutkowska G., Iwaszko M. (2015) Effect of fly ash from the incineration of sewage sludge on the strength and frost resistance of fine-grained concrete, Inzynieria Ekologiczna, Ecological Engineering 45, 59-67. DOI: 10.12912/23920629/60595 (in Polish).10.12912/23920629/60595
  17. Szarek Ł. (2016) The ash from thermal utilization of sewage sludge and PN-EN 450-1:2012 (Dean’s grant report No. 504/02102) (unpublished),Warsaw University of Technology, Faculty of Building Services, Hydro and Environmental Engineering, Warszawa (in Polish).
  18. Technical approval ITP (2011) AT/18-2011-0052-00, Inst. Technologiczno-Przyrodniczy, Falenty (in Polish).
  19. Twardowski K., Drozdzak R. (2007) Determining ground water-tightness in laboratory conditions, Wiertnictwo Nafta Gaz, 24 (1), 565-574 (in Polish).
  20. Updating the National Waste Management Plan 2014 (2015) Warszawa (in Polish).
DOI: https://doi.org/10.1515/heem-2016-0004 | Journal eISSN: 2300-8687 | Journal ISSN: 1231-3726
Language: English
Page range: 47 - 61
Submitted on: Apr 7, 2016
Published on: Sep 20, 2016
Published by: Polish Academy of Sciences, Institute of Hydro-Engineering
In partnership with: Paradigm Publishing Services
Publication frequency: 2 issues per year

© 2016 Paweł Falacinski, Łukasz Szarek, published by Polish Academy of Sciences, Institute of Hydro-Engineering
This work is licensed under the Creative Commons Attribution-NonCommercial-NoDerivatives 4.0 License.