Experimental Procedure Used To Determine The Flexural Rigidity For Composite Sandwich Bars With Various Thickness Values Cover

Experimental Procedure Used To Determine The Flexural Rigidity For Composite Sandwich Bars With Various Thickness Values

Open Access
|Sep 2015

References

  1. 1. Oya, A., Kasahara, N., Horigome, R., Structure of porous carbon-fiber from phenolic polymer containing polystyrene microbeads,, Vol. 20, pp. 409-411, (2001).
  2. 2. Lukyanov, A., A., Effect of fiber orientation on the structure of shock waves in carbon fiber-epoxy composites,, Vol. 47, No. 6, pp. 617-626, (2012).
  3. 3. Stănescu, N., M., Bolcu, D., Pastramă, S., D., Ciucă, I., Manea, I., Baciu, F., Determination of damping factor, to vibrations of composite bars, reinforced with carbon and kevlar texture,Vol. 47, No. 4, pp. 492-496, (2010).
  4. 4. Burada, C., O., Miriţoiu, C., M., Bolcu, D., Stănescu, M., M., Experimental determinations of the damping factor and stiffness for new sandwich platbands with different reinforcement and core,, Vol. 44, No. 4, pp. 405-413, (2014).
  5. 5. Voicu, R., Structural characterization and mechanical behaviour of carbon fiber/epoxy composites for aeronautical field,Vol. 49, No. 1, pp. 34-40, (2012).
  6. 6. Burada, C., Determinări practice în laboratoarele de analiză şi încercări pentru construcţii, Universitaria, Craiova, (2010).
  7. 7. Burada, C., Încercări de laborator pentru materiale de construcţii, Universitaria, Craiova, (2011).
  8. 8. Kamae, T., Drzal, L., T., Carbon fiber/epoxy composite property enhacement through incorporation of carbon nanotubes at the fiber-matrix interphase- Part I: The development of carbon nanotube coated carbon fibers and the evaluation of their adhesion,, Vol. 43, No. 9, pp. 1569-1577, (2012).
  9. 9. Kumar, B., G., Singh, R., P., Nakamura, T., Degradation of carbon fiber-reinforced epoxy composites by ultraviolet radiation and condensation,, Vol. 36, No. 24, pp. 2713-2721, (2002).
  10. 10. Baurova, N., I., Surface structure of fractured carbon-fiber composites before and after climatic aging,, Vol. 46, No. 4, pp. 241-244, (2014).
DOI: https://doi.org/10.1515/aucts-2015-0056 | Journal eISSN: 2668-6449 (formerly 1583-7149) | Journal ISSN: 1583-7149
Language: English
Page range: 7 - 12
Published on: Sep 23, 2015
Published by: Lucian Blaga University of Sibiu
In partnership with: Paradigm Publishing Services
Publication frequency: 1 issue per year

© 2015 Cosmin Mihai Miriţoiu, published by Lucian Blaga University of Sibiu
This work is licensed under the Creative Commons Attribution-NonCommercial-NoDerivatives 3.0 License.