Have a personal or library account? Click to login

Delamination Resistance Of Laminate Made With VBO MTM46/HTS Prepreg

Open Access
|Nov 2015

Abstract

A laminate made with the Vacuum Bag Only (VBO) prepregs can be cured out of autoclave. Because of low curing pressure such a process can result in deterioration of laminate mechanical properties. They can be significantly lower than those displayed by the autoclave cured ones. The resistance against delamination can be among the most affected. Since this property is a week point of all the laminates it was of particular interest. Delamination resistance of unidirectional laminate made from VBO MTM46/HTS(12K) prepreg was in the scope of the presented research and the critical values of the Strain Energy Release Rates and the Paris-type equations corresponding to Mode I, Mode II and Mixed-Mode I/II static and cyclic loadings, respectively, were determined.

DOI: https://doi.org/10.1515/ama-2015-0029 | Journal eISSN: 2300-5319 | Journal ISSN: 1898-4088
Language: English
Page range: 173 - 177
Submitted on: May 4, 2015
Accepted on: Oct 29, 2015
Published on: Nov 7, 2015
Published by: Bialystok University of Technology
In partnership with: Paradigm Publishing Services
Publication frequency: 4 times per year

© 2015 Piotr Czarnocki, Kamila Czajkowska, published by Bialystok University of Technology
This work is licensed under the Creative Commons Attribution-NonCommercial-NoDerivatives 3.0 License.